spezifischer Widerstand: 2.95E-7 Ω·m

Quick Comparison

Kohlenstoffarmer Stahl

EN 10025-2 Grade S235JR as-rolled condition (+AR)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Molybdenum Steel

EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Kohlenstoffarmer Stahl

EN 10025-2 Grade S185 normalized or normalized formed (+N)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00
Seite 1 von 17