Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Austenitischer rostfreier Stahl
Sandvik 253 MAGeliefert von:
Alleima (formerly Sandvik Materials Technology)Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Austenitischer rostfreier Stahl
EN 10088-1 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Ferritischer Edelstahl
DIN 17440 Grade X6CrAl13 soft annealed (+A)Austenitischer rostfreier Stahl
EN 10088-1 Grade X1CrNi25-21 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X8CrNiNb16-13 solution annealed (+AT)Ferritischer Edelstahl
EN 10088-1 Grade X6CrAl13 soft annealed (+A)Austenitischer rostfreier Stahl
EN 10028-7 Grade X1CrNi25-21 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X1CrNi25-21 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Grey Cast Iron
EN 1561 Grade GJL-350 cast conditionMartensitischer Edelstahl
SEW 400 Grade X4CrNi13-4 quenched and tempered (+QT1)Austenitischer rostfreier Stahl
EN 10216-5 Grade X8CrNiNb16-13 solution annealed (+AT)Martensitischer Edelstahl
EN 10272 Grade X3CrNiMo13-4 quenched and tempered (+QT780)Martensitischer Edelstahl
EN 10272 Grade X3CrNiMo13-4 quenched and tempered (+QT650)