General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Density | 1.34 - 1.35 g/cm³ Show Supplier Material materials with Density of 1.34 - 1.35 g/cm³ | Depending on the thickness of the specimen | |
Moisture absorption | 1.1 % Show Supplier Material materials with Moisture absorption of 1.1 % | ASTM D348 |
Mechanical
Property | Value | Comment |
---|---|---|
Compressive modulus | 4.1 GPa Show Supplier Material materials with Compressive modulus of 4.1 GPa | |
Compressive strength | 137.9 MPa Show Supplier Material materials with Compressive strength of 137.9 MPa | |
Flexural modulus | 3.5 - 5.2 GPa Show Supplier Material materials with Flexural modulus of 3.5 - 5.2 GPa | Minimum value for ISSC |
Flexural strength | 60 - 75.8 MPa Show Supplier Material materials with Flexural strength of 60 - 75.8 MPa | Minimum value for ISSC |
Hardness, Rockwell M | 70 [-] Show Supplier Material materials with Hardness, Rockwell M of 70 [-] | |
Tensile strength | 37.9-51 | Depending on the thickness of the specimen |
Thermal
Property | Value | Comment |
---|---|---|
Relative temperature index, mechanical strength | 165 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 165 °C | ¹ |
Technological properties
Property | ||
---|---|---|
Application areas | It is used as a bearing material or in other wear applications. | |
Fillers | Aramid Fiber | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |