Nickel Steel
EN 10028-4 Grade 11MnNi5-3 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Nickel Steel
EN 10028-4 Grade 12Ni14 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Nickel Steel
EN 10028-4 Grade 13MnNi6-3 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Nickel Steel
EN 10028-4 Grade 15NiMn6 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Martensitischer Edelstahl
ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)Geliefert von:
1 Matmatch-Lieferant
Austenitischer rostfreier Stahl
ASTM A276 Grade S20910 AnnealedAustenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMoN17-13-5 solution annealed (+AT)