Kohlenstoffarmer Stahl
EN 10028-2 Grade P355GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 12CrMo9-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Nickel Molybdenum Steel
EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 12CrMoV12-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoSi5-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoV9-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Nickel molybdenum Steel
EN 10028-2 Grade 15NiCuMoNb5-6-4 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Molybdenum Steel
EN 10028-2 Grade 18MnMo4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-5 Grade S355J2W normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-5 Grade S355K2W normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Chromium Molybdenum Steel
EN 10216-2 Grade 12CrMo9-10 quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10216-2 Grade 19Mn5 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10217-3 Grade WStE 355 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17179 Grade WStE 355 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 1628 Grade St 52.4 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10216-3 Grade P355NH normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10217-3 Grade EStE 355 normalized or normalized formed (+N)