Martensitischer Edelstahl
DIN 17440 Grade X12Cr13 soft annealed (+A)Martensitischer Edelstahl
EN 10088-1 Grade X6Cr13 soft annealed (+A)Ferritischer Edelstahl
EN 10088-1 Grade X2CrTi17 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X6Cr13 soft annealed (+A)Ferritischer Edelstahl
DIN 17456 Grade X2CrTi12 soft annealed (+A)Ferritischer Edelstahl
EN 10028-7 Grade X2CrTi17 soft annealed (+A)Ferritischer Edelstahl
EN 10312 Grade X2CrTi12 soft annealed (+A)Ferritischer Edelstahl
EN 10088-4 Grade X2CrTi12 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X10Cr13 quenched and tempered (+QT)Ferritischer Edelstahl
DIN 17441 Grade X6CrTi12 soft annealed (+A)Chromium Molybdenum Steel
EN 10216-2 Grade 20CrMoV13-5 quenched and tempered (+QT)Chromium Molybdenum Steel
EN 10216-2 Grade 20CrMoV13-5-5 quenched and tempered (+QT)Martensitischer Edelstahl
DIN 1654-5 Grade X10Cr13 quenched and tempered (+QT)Chromium Molybdenum Steel
DIN 17240 Grade 21CrMoV5-7 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10083-1 Grade 30CrNiMo8 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10083-1 Grade 34CrNiMo6 quenched and tempered (+QT)Martensitischer Edelstahl
EN 10088-1 Grade X12Cr13 quenched and tempered (+QT650)Chromium Molybdenum Steel
EN 10277-5 Grade 30CrMoV9 cold drawn or turned and quenched and temperedNickel Chromium Molybdenum Steel
EN 10277-5 Grade 30CrNiMo8 cold drawn or turned and quenched and temperedNickel Chromium Molybdenum Steel
EN 10277-5 Grade 34CrNiMo6 cold drawn or turned and quenched and tempered