Austenitischer rostfreier Stahl
ASTM A193 Grade B8MN Class 1D, Carbide solution treatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8MN Class 1B, Carbide solution treatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8N Class 1B, Carbide solution treatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8N Class 1D, Carbide solution treatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8MLCuN Class 1B, Carbide solution treatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8MLCuN Class 1D, Carbide solution treatedMartensitischer Edelstahl
ASTM A487 Grade CA15 Class D, Heat-TreatedMedium Carbon Steel
ASTM A372 Grade G Class 70, Normalized, Normalized and Tempered, Liquid Quenched and Tempered, or Normalized followed by Liquid Quench and TemperMartensitischer Edelstahl
ASTM A487 Grade CA15M Class A, Heat-TreatedMartensitischer Edelstahl
ASTM A487 Grade CA6NM Class A, Heat-TreatedAustenitischer rostfreier Stahl
ASTM A487 Grade 8 Class A, Heat-TreatedMartensitischer Edelstahl
ASTM A487 Grade 7 Class A, Heat-TreatedNickel Chromium Molybdenum Steel
ASTM A372 Grade L Liquid Quenched and Tempered, or Normalized followed by Liquid Quench and TemperNickel Molybdenum Steel
ASTM A487 Grade 11 Class A, Heat-TreatedNickel Molybdenum Steel
ASTM A487 Grade 11 Class B, Heat-TreatedNickel Chromium Iron Alloy
ASTM A240 Grade N08020 Heat-TreatedManganese Steel
ASTM A487 Grade 1 Class C, Heat-TreatedNickel Chromium Molybdenum Steel
ASTM A487 Grade 2 Class C, Heat-TreatedNickel Chromium Iron Alloy
ASTM A182 Grade F20 Solution-Annealed