ASTM A372 Grade G Class 70, Normalized, Normalized and Tempered, Liquid Quenched and Tempered, or Normalized followed by Liquid Quench and Temper

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Medium Carbon Steel

Mechanical

PropertyTemperatureValueComment

Elongation A50

20.0 °C

0 - 18 %

Show Material materials with Elongation A50 of 0 - 18 %

Hardness, Brinell

20.0 °C

0 - 248 [-]

Show Material materials with Hardness, Brinell of 0 - 248 [-]

Poisson's ratio

20.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Medium Carbon Steel

Shear modulus

20.0 °C

75 - 80 GPa

Show Material materials with Shear modulus of 75 - 80 GPa

Typical for Carbon Steel

Tensile strength

20.0 °C

825 - 1000 MPa

Show Material materials with Tensile strength of 825 - 1000 MPa

Yield Strength Rp0.2, short transverse

20.0 °C

0 - 485 MPa

Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 485 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K

Typical for Carbon Steel

Melting point

1425 - 1514 °C

Show Material materials with Melting point of 1425 - 1514 °C

Typical for Medium Carbon Steel

Chemical properties

PropertyValue

Carbon

0.25 - 0.35 %

Show Material materials with Carbon of 0.25 - 0.35 %

Chromium

0.4 - 0.65 %

Show Material materials with Chromium of 0.4 - 0.65 %

Manganese

0.7 - 1 %

Show Material materials with Manganese of 0.7 - 1 %

Molybdenum

0.15 - 0.25 %

Show Material materials with Molybdenum of 0.15 - 0.25 %

Phosphorus

0 - 0.02 %

Show Material materials with Phosphorus of 0 - 0.02 %

Silicon

0.15 - 0.35 %

Show Material materials with Silicon of 0.15 - 0.35 %

Sulfur

0 - 0.01 %

Show Material materials with Sulfur of 0 - 0.01 %