ASTM A487 Grade CA15M Class A, Heat-Treated

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

7.6 - 7.7 g/cm³

Show Material materials with Density of 7.6 - 7.7 g/cm³

Typical for Martensitic Stainless Steel

Mechanical

PropertyTemperatureValueComment

Elongation A50

20.0 °C

0 - 18 %

Show Material materials with Elongation A50 of 0 - 18 %

Poisson's ratio

20.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Martensitic Stainless Steel

Reduction of area

20.0 °C

0 - 30 %

Show Material materials with Reduction of area of 0 - 30 %

Tensile strength

20.0 °C

0 - 620 MPa

Show Material materials with Tensile strength of 0 - 620 MPa

Yield Strength Rp0.2, short transverse

20.0 °C

0 - 450 MPa

Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 450 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1E-5 - 1.5E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1E-5 - 1.5E-5 1/K

Typical for Martensitic Stainless Steel

Melting point

1375 - 1450 °C

Show Material materials with Melting point of 1375 - 1450 °C

Typical for Martensitic Stainless Steel

Thermal conductivity

20.0 °C

14 - 31 W/(m·K)

Show Material materials with Thermal conductivity of 14 - 31 W/(m·K)

Typical for Martensitic Stainless Steel

Chemical properties

PropertyValue

Carbon

0 - 0.15 %

Show Material materials with Carbon of 0 - 0.15 %

Copper

0 - 0.1 %

Show Material materials with Copper of 0 - 0.1 %

Manganese

0 - 1 %

Show Material materials with Manganese of 0 - 1 %

Molybdenum

0.15 - 1 %

Show Material materials with Molybdenum of 0.15 - 1 %

Nickel

0 - 0.05 %

Show Material materials with Nickel of 0 - 0.05 %

Phosphorus

0 - 0.04 %

Show Material materials with Phosphorus of 0 - 0.04 %

Silicon

0 - 0.65 %

Show Material materials with Silicon of 0 - 0.65 %

Sulfur

0 - 0.035 %

Show Material materials with Sulfur of 0 - 0.035 %