Kohlenstoffarmer Stahl
EN 10025-2 Grade S235J2 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-2 Grade S235JR as-rolled condition (+AR)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade S235J0 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade S185 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025 Grade S235JRG2C as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S235J0C as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S235J2G3 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 5512-1 Grade S235J2G3 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 5512-1 Grade S235JRG2 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10025 Grade S235JRG1 as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade RSt 37-2 untreatedKohlenstoffarmer Stahl
EN 10277-2 Grade RSt 37-2 cold drawnKohlenstoffarmer Stahl
EN 10277-2 Grade RSt 37-2 cold drawn or turned and normalizedKohlenstoffarmer Stahl
EN 10277-2 Grade RSt 37-2 turnedKohlenstoffarmer Stahl
EN 10277-2 Grade St 37-3 cold drawnKohlenstoffarmer Stahl
EN 10277-2 Grade St 37-3 cold drawn or turned and normalizedKohlenstoffarmer Stahl
EN 10277-2 Grade St 37-3 turnedKohlenstoffarmer Stahl
DIN 2393-2 Grade RSt 37-2 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 2393-2 Grade RSt 37-2 bright drawn and stress relievedKohlenstoffarmer Stahl
EN 10305-3 Grade RSt 37-2 normalized or normalized formed (+N)