Nickel Chromium Iron Alloy
DIN 17744 Grade NiCr19NbMo precipitation hardened (+P)Nickel Chromium Iron Alloy
DIN 17744 Grade NiCr21Mo soft annealed (+A)Nickel Chromium Molybdenum Alloy
DIN 17744 Grade NiCr22Mo9Nb soft annealed (+A)Nickel Chromium Cobalt Alloy
DIN 17744 Grade NiCo20Cr20MoTi precipitation hardened (+P)Nickel Molybdenum Alloy
DIN 17744 Grade NiMo28 solution annealed (+AT)Nickel Chromium Iron Alloy
DIN 17744 Grade NiCr20CuMo stabilizedNickel Chromium Molybdenum Alloy
DIN 17744 Grade NiMo16Cr16Ti solution heat-treated and quenchedNickel Chromium Alloy
DIN 17744 Grade NiCr22Mo7Cu solution annealed (+AT)Nickel Chromium Molybdenum Alloy
DIN 17744 Grade NiMo23Cr8Fe solution annealed (+AT)Nickel Chromium Alloy
DIN 17744 Grade NiCr21Mo6CuNickel Chromium Alloy
DIN 17744 Grade NiCr22Mo6CuNickel Chromium Molybdenum Alloy
DIN 17744 Grade NiMo16Cr15W solution heat-treated and quenchedNickel Molybdenum Alloy
DIN 17744 Grade 2.4600Nickel Chromium Iron Alloy
DIN 17744 Grade 2.4608Nickel Molybdenum Alloy
DIN 17744 Grade 2.4617Nickel Chromium Alloy
DIN 17744 Grade 2.4619Nickel Chromium Iron Alloy
DIN 17744 Grade 2.4668Nickel Chromium Iron Alloy
DIN 17744 Grade 2.4660Nickel Chromium Alloy
DIN 17744 Grade 2.4665Nickel Chromium Iron Alloy
DIN 17744 Grade 2.4858