Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 1.41 g/cm³ Show Supplier Material materials with Dichte of 1.41 g/cm³ | ISO 1183 |
Moisture absorption | 20.0 °C | 2.65 % Show Supplier Material materials with Moisture absorption of 2.65 % | ISO 62, after 24h |
Sauerstoffindex | 20.0 °C | 20 % Show Supplier Material materials with Sauerstoffindex of 20 % | ISO 4589-1/-2 |
Viscosity number | 145 cm³/gr Show Supplier Material materials with Viscosity number of 145 cm³/gr | ISO 307, 1157, 1628 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 20.0 °C | 300 MPa Show Supplier Material materials with Biegefestigkeit of 300 MPa | ISO 178 |
120.0 °C | 160 MPa Show Supplier Material materials with Biegefestigkeit of 160 MPa | ISO 178 | |
160.0 °C | 130 MPa Show Supplier Material materials with Biegefestigkeit of 130 MPa | ISO 178 | |
Biegemodul | 20.0 °C | 9 GPa Show Supplier Material materials with Biegemodul of 9 GPa | ISO 178 |
120.0 °C | 4.7 GPa Show Supplier Material materials with Biegemodul of 4.7 GPa | ISO 178 | |
160.0 °C | 3.9 GPa Show Supplier Material materials with Biegemodul of 3.9 GPa | ISO 178 | |
Dehnung | 20.0 °C | 4 % Show Supplier Material materials with Dehnung of 4 % | ISO 527-1/-2 |
120.0 °C | 7.5 % Show Supplier Material materials with Dehnung of 7.5 % | ISO 527-1/-2 | |
160.0 °C | 7.5 % Show Supplier Material materials with Dehnung of 7.5 % | ISO 527-1/-2 | |
180.0 °C | 7.5 % Show Supplier Material materials with Dehnung of 7.5 % | ISO 527-1/-2 | |
200.0 °C | 7.5 % Show Supplier Material materials with Dehnung of 7.5 % | ISO 527-1/-2 | |
Elastizitätsmodul | 20.0 °C | 10 GPa Show Supplier Material materials with Elastizitätsmodul of 10 GPa | ISO 527-1/-2 |
120.0 °C | 5.5 GPa Show Supplier Material materials with Elastizitätsmodul of 5.5 GPa | ISO 527-1/-2 | |
160.0 °C | 5 GPa Show Supplier Material materials with Elastizitätsmodul of 5 GPa | ISO 527-1/-2 | |
180.0 °C | 4.4 GPa Show Supplier Material materials with Elastizitätsmodul of 4.4 GPa | ISO 527-1/-2 | |
200.0 °C | 4 GPa Show Supplier Material materials with Elastizitätsmodul of 4 GPa | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 11 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m² | ISO 179/1eU |
23.0 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | ISO 179/1eU | |
Schlagzähigkeit, Charpy ungekerbt | -30.0 °C | 65 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 65 kJ/m² | ISO 179/1eU |
23.0 °C | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | ISO 179/1eU | |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 11 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 11 kJ/m² | ISO 180/1A |
23.0 °C | 12 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 12 kJ/m² | ISO 180/1A | |
Zugfestigkeit | 20.0 °C | 210 MPa Show Supplier Material materials with Zugfestigkeit of 210 MPa | ISO 527-1/-2 |
120.0 °C | 110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | ISO 527-1/-2 | |
160.0 °C | 100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | ISO 527-1/-2 | |
180.0 °C | 95 MPa Show Supplier Material materials with Zugfestigkeit of 95 MPa | ISO 527-1/-2 | |
200.0 °C | 90 MPa Show Supplier Material materials with Zugfestigkeit of 90 MPa | ISO 527-1/-2 | |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | |||
Ball pressure temperature | 285 °C Show Supplier Material materials with Ball pressure temperature of 285 °C | ||||
Heat deflection temperature, 0.45 MPa | 290 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 290 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 290 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 290 °C | ISO 75-1/-2 | |||
Koeffizient der thermischen Ausdehnung | 20.0 °C | 2.5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-5 1/K | ISO 11359-1/-2 | ||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | UL 746B, Thickness 0.9, 3mm | |||
Relative temperature index, mechanical impact | 120140 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120140 °C | UL 746B, respectively for 0.9 and 3mm thickness | |||
Relative temperature index, mechanical strength | 120140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120140 °C | UL 746B, respectively for 0.9 and 3mm thickness | |||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | ISO 11357-1/-3, 10°C/min | |||
Vicat-Erweichungstemperatur | 290 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 290 °C | ISO 306, 50°C/h 50N | |||
thermischer Ausdehnungskoeffizient, transversal | 20.0 °C | 6E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6E-5 1/K | ISO 11359-1/-2 | ||
Entflammbarkeit | for thickness 1.5 and 0.75mm: HB, UL recognition: Yes, IEC 60695-11-10 | ||||
Glow Wire Flammability Index (GWFI) | 960°C at 3mm and 650°C at 0.75mm, IEC 60695-2-1 | ||||
Glow Wire Ignition Temperature (GWIT) | 725°C at 3mm and. 700°C at 0.75mm, IEC 60695-2-13 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 20.0 °C | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 4 [-] | IEC 60250 |
Dielektrizitätskonstante, 100 Hz | 20.0 °C | 4.3 [-] Show Supplier Material materials with Dielektrizitätskonstante, 100 Hz of 4.3 [-] | IEC 60250 |
Dissipation factor, 100Hz | 20.0 °C | 7E-3 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 7E-3 [-] | IEC 60250 |
Dissipation factor, 1MHz | 20.0 °C | 0.02 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.02 [-] | IEC 60250 |
Durchschlagfestigkeit | 20.0 °C | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | IEC 60243-1 |
Kriechstromfestigkeit | 20.0 °C | 300 V Show Supplier Material materials with Kriechstromfestigkeit of 300 V | IEC 60112 |
spezifischer Widerstand | 20.0 °C | 1.00E+14 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+14 Ω·m | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Density of melt | 1.21 g/cm³ Show Supplier Material materials with Density of melt of 1.21 g/cm³ | ||||
Eff. thermal diffusivity | 0.11 mm²/s Show Supplier Material materials with Eff. thermal diffusivity of 0.11 mm²/s | ||||
Schrumpfung | 20.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | Sim. to ISO 294-4 | ||
Schrumpfung, diagonal | 20.0 °C | 1.3 % Show Supplier Material materials with Schrumpfung, diagonal of 1.3 % | Sim. to ISO 294-4 | ||
Specific heat capacity melt | 2200 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2200 J/(kg·K) | ||||
Thermal conductivity of melt | 0.3 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.3 W/(m·K) | ||||
Spiral flow length | 1.0 mm 800 bar: 100mm, 1.0 mm 900 bar: 110mm, 1.0 mm 1000 bar: 120mm, 0.5mm 1200 bar: 33mm, 0.5 mm 1600 bar: 44mm, 0.5 mm 2000 bar: 76mm |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive Bearing Cages, Automotive Connectors, Automotive e-motor Bobbins, Bobbins, Brushholders (electrical components), Brushholders (electro motors), Charge Air Cooler Caps, Coil insulation, DRL sockets, E-Boxes, E-motor electric insulation, Endlaminates (electro motors), Fuse Holders, Hot Charged Air Ducts, Lawnmower Muffler Components, Lawnmower Trimmer Muffler, MTF/DMF Components, Positition Sensor, Self propelled lawnmower transmission gears, Speed Sensor, Start/Stop: Alternator and Starter parts, Suspension System Top Mounts, Temperature Sensor, Torque Convertor Components | |
Fillers | 30% Glass Fiber |