Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.41 g/cm³ Show Supplier Material materials with Dichte of 1.41 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Wasserabsorption | 5.5 % Show Supplier Material materials with Wasserabsorption of 5.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 7.5 GPa Show Supplier Material materials with Biegemodul of 7.5 GPa | conditioned | ISO 178 | |
11 GPa Show Supplier Material materials with Biegemodul of 11 GPa | dry | ISO 178 | ||
Dehnung | -40 °C | 3.3 % Show Supplier Material materials with Dehnung of 3.3 % | dry | ISO 527-1/-2 |
3.5 % Show Supplier Material materials with Dehnung of 3.5 % | dry | ISO 527-1/-2 | ||
5.8 % Show Supplier Material materials with Dehnung of 5.8 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | -40 °C | 12 GPa Show Supplier Material materials with Elastizitätsmodul of 12 GPa | dry | ISO 527-1/-2 |
7.5 GPa Show Supplier Material materials with Elastizitätsmodul of 7.5 GPa | conditioned | ISO 527-1/-2 | ||
11.5 GPa Show Supplier Material materials with Elastizitätsmodul of 11.5 GPa | dry | ISO 527-1/-2 | ||
100 °C | 5.7 GPa Show Supplier Material materials with Elastizitätsmodul of 5.7 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 210 MPa Show Supplier Material materials with Flexural yield strength of 210 MPa | conditioned | ISO 178 | |
310 MPa Show Supplier Material materials with Flexural yield strength of 310 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry | ISO 179/1eA |
-30 °C | 11 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 12.8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12.8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 18 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 18 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 74 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 74 kJ/m² | conditioned | ISO 179/1eU |
-30 °C | 75 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 75 kJ/m² | dry | ISO 179/1eU | |
23 °C | 90 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 90 kJ/m² | dry | ISO 179/1eU | |
23 °C | 95 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 95 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | -40 °C | 270 MPa Show Supplier Material materials with Zugfestigkeit of 270 MPa | dry | ISO 527-1/-2 |
140 MPa Show Supplier Material materials with Zugfestigkeit of 140 MPa | conditioned | ISO 527-1/-2 | ||
210 MPa Show Supplier Material materials with Zugfestigkeit of 210 MPa | dry | ISO 527-1/-2 | ||
100 °C | 120 MPa Show Supplier Material materials with Zugfestigkeit of 120 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 250 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 250 °C | dry | ISO 75-1/-2 | 2 MPa | |
260 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 260 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 35% Glass Fiber |