Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.46 g/cm³ Show Supplier Material materials with Dichte of 1.46 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 | |
Sauerstoffindex | 39 % Show Supplier Material materials with Sauerstoffindex of 39 % | dry | ISO 4589-1/-2 | |
Wasserabsorption | 0.3 % Show Supplier Material materials with Wasserabsorption of 0.3 % | dry | ISO 62 | at 23°C after 24h |
4.1 % Show Supplier Material materials with Wasserabsorption of 4.1 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Biegemodul | 11 GPa Show Supplier Material materials with Biegemodul of 11 GPa | dry | ISO 178 | |||
11.5 GPa Show Supplier Material materials with Biegemodul of 11.5 GPa | conditioned | ISO 178 | ||||
80 °C | 7.6 GPa Show Supplier Material materials with Biegemodul of 7.6 GPa | conditioned | ISO 178 | |||
80 °C | 10.5 GPa Show Supplier Material materials with Biegemodul of 10.5 GPa | dry | ISO 178 | |||
120 °C | 8.2 GPa Show Supplier Material materials with Biegemodul of 8.2 GPa | dry | ISO 178 | |||
160 °C | 5 GPa Show Supplier Material materials with Biegemodul of 5 GPa | dry | ISO 178 | |||
Dehnung | -40 °C | 2.2 % Show Supplier Material materials with Dehnung of 2.2 % | dry | ISO 527-1/-2 | ||
1.9 % Show Supplier Material materials with Dehnung of 1.9 % | conditioned | ISO 527-1/-2 | ||||
2 % Show Supplier Material materials with Dehnung of 2 % | dry | ISO 527-1/-2 | ||||
2.1 % Show Supplier Material materials with Dehnung of 2.1 % | dry | ISO 527-1/-2 | 1 mm | |||
40 °C | 1.9 % Show Supplier Material materials with Dehnung of 1.9 % | dry | ISO 527-1/-2 | |||
80 °C | 1.9 % Show Supplier Material materials with Dehnung of 1.9 % | dry | ISO 527-1/-2 | |||
80 °C | 2.9 % Show Supplier Material materials with Dehnung of 2.9 % | conditioned | ISO 527-1/-2 | |||
100 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | dry | ISO 527-1/-2 | |||
120 °C | 2.6 % Show Supplier Material materials with Dehnung of 2.6 % | dry | ISO 527-1/-2 | |||
140 °C | 3.3 % Show Supplier Material materials with Dehnung of 3.3 % | dry | ISO 527-1/-2 | |||
160 °C | 3.8 % Show Supplier Material materials with Dehnung of 3.8 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | -40 °C | 12 GPa Show Supplier Material materials with Elastizitätsmodul of 12 GPa | dry | ISO 527-1/-2 | ||
10.7 GPa Show Supplier Material materials with Elastizitätsmodul of 10.7 GPa | dry | ISO 527-1/-2 | 1 mm | |||
11.5 GPa Show Supplier Material materials with Elastizitätsmodul of 11.5 GPa | dry | ISO 527-1/-2 | ||||
12 GPa Show Supplier Material materials with Elastizitätsmodul of 12 GPa | conditioned | ISO 527-1/-2 | ||||
40 °C | 11.3 GPa Show Supplier Material materials with Elastizitätsmodul of 11.3 GPa | dry | ISO 527-1/-2 | |||
80 °C | 7.6 GPa Show Supplier Material materials with Elastizitätsmodul of 7.6 GPa | conditioned | ISO 527-1/-2 | |||
80 °C | 10.8 GPa Show Supplier Material materials with Elastizitätsmodul of 10.8 GPa | dry | ISO 527-1/-2 | |||
100 °C | 10 GPa Show Supplier Material materials with Elastizitätsmodul of 10 GPa | dry | ISO 527-1/-2 | |||
120 °C | 8 GPa Show Supplier Material materials with Elastizitätsmodul of 8 GPa | dry | ISO 527-1/-2 | |||
140 °C | 5.7 GPa Show Supplier Material materials with Elastizitätsmodul of 5.7 GPa | dry | ISO 527-1/-2 | |||
160 °C | 5 GPa Show Supplier Material materials with Elastizitätsmodul of 5 GPa | dry | ISO 527-1/-2 | |||
Flexural yield strength | 220 MPa Show Supplier Material materials with Flexural yield strength of 220 MPa | conditioned | ISO 178 | |||
245 MPa Show Supplier Material materials with Flexural yield strength of 245 MPa | dry | ISO 178 | ||||
80 °C | 130 MPa Show Supplier Material materials with Flexural yield strength of 130 MPa | conditioned | ISO 178 | |||
80 °C | 190 MPa Show Supplier Material materials with Flexural yield strength of 190 MPa | dry | ISO 178 | |||
120 °C | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | |||
160 °C | 100 MPa Show Supplier Material materials with Flexural yield strength of 100 MPa | dry | ISO 178 | |||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 7.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7.5 kJ/m² | dry, conditioned | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | dry, conditioned | ISO 179/1eU | ||
Zugfestigkeit | -40 °C | 175 MPa Show Supplier Material materials with Zugfestigkeit of 175 MPa | dry | ISO 527-1/-2 | ||
140 MPa Show Supplier Material materials with Zugfestigkeit of 140 MPa | conditioned | ISO 527-1/-2 | ||||
150 MPa Show Supplier Material materials with Zugfestigkeit of 150 MPa | dry | ISO 527-1/-2 | ||||
160 MPa Show Supplier Material materials with Zugfestigkeit of 160 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness | ||
40 °C | 145 MPa Show Supplier Material materials with Zugfestigkeit of 145 MPa | dry | ISO 527-1/-2 | |||
80 °C | 85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | conditioned | ISO 527-1/-2 | |||
80 °C | 125 MPa Show Supplier Material materials with Zugfestigkeit of 125 MPa | dry | ISO 527-1/-2 | |||
100 °C | 115 MPa Show Supplier Material materials with Zugfestigkeit of 115 MPa | dry | ISO 527-1/-2 | |||
120 °C | 100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | dry | ISO 527-1/-2 | |||
140 °C | 80 MPa Show Supplier Material materials with Zugfestigkeit of 80 MPa | dry | ISO 527-1/-2 | |||
160 °C | 70 MPa Show Supplier Material materials with Zugfestigkeit of 70 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 305 °C Show Supplier Material materials with Ball pressure temperature of 305 °C | dry | IEC 60695-10-2 | |||
Entflammbarkeit | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
V-0 | dry | IEC 60695-11-10 | 0.2 mm | UL recognition :Yes | ||
Glasübergangstemperatur | 125 °C Show Supplier Material materials with Glasübergangstemperatur of 125 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.25 mm | |||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 3 mm | ||
800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 0.75 mm | |||
Koeffizient der thermischen Ausdehnung | 2e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | dry | UL746B | 0.35 mm | ||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | dry | UL746B | 0.35 mm | ||
Schmelzpunkt | 325 °C Show Supplier Material materials with Schmelzpunkt of 325 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 305 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 305 °C | dry | ISO 75-1/-2 | 2 MPa | ||
323 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 323 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Wärmeleitfähigkeit | 0.4 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.4 W/(m·K) | dry | ASTM E1461 | in plane |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.8 [-] | dry | IEC 60250 | 1GHz |
3.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.8 [-] | dry | IEC 60250 | 10GHz | |
3.9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.9 [-] | dry, conditioned | IEC 62631-2-1 | 1MHz | |
3.9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.9 [-] | conditioned | IEC 60250 | 1GHz | |
3.9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.9 [-] | conditioned | IEC 60250 | 10GHz | |
4.2 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.2 [-] | dry, conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 33 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 33 kV/mm | dry, conditioned | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 64 [-] Show Supplier Material materials with Verlustfaktor of 64 [-] | dry, conditioned | IEC 62631-2-1 | 100Hz |
110 [-] Show Supplier Material materials with Verlustfaktor of 110 [-] | dry | IEC 60250 | 10GHz | |
130 [-] Show Supplier Material materials with Verlustfaktor of 130 [-] | dry, conditioned | IEC 60250 | 1GHz | |
130 [-] Show Supplier Material materials with Verlustfaktor of 130 [-] | conditioned | IEC 60250 | 10GHz | |
176 [-] Show Supplier Material materials with Verlustfaktor of 176 [-] | dry, conditioned | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry, conditioned | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.35 % Show Supplier Material materials with Schrumpfung of 0.35 % | dry | ISO 294-4 | Parallel |
1.2 % Show Supplier Material materials with Schrumpfung of 1.2 % | dry | ISO 294-4 | Normal | |
Spiral flow length | 110 | dry | - | 1.0 mm 800 bar |
120 | dry | - | 1.0 mm 900 bar | |
130 | dry | - | 1.0 mm 1000 bar | |
Viscosity number | 86 cm³/gr Show Supplier Material materials with Viscosity number of 86 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Miniature Circuit Breakers, Reflow connectors, FPC connectors, WtB and BtB Connectors, Battery Connectors, Endlaminates (electro motors), Brushholders (electro motors), Coil insulation, Automotive e-motor Bobbins, Temperature Sensor, Speed Sensor, Positition Sensor, EGR sensor, Start/Stop: Alternator and Starter parts, HDMI Connectors, Molded case circuit breakers, MCCB Housings, Industrial Control Gear, Contactors, Motor Starter/Overload Relays, Medium Voltage Circuit Breakers, Medium Voltage Circuit Breaker Isolators, Reflow connectors (2), Reflow connectors (3), Fuse holder, Micro appliance connector, High voltage connector e-motor | |
Certifications | VDE, Yellow Card Available | |
Fillers | 30% Glass Fiber |