EcoPaXX® Q170E-H B-MB

Want to keep this datasheet? Save it now in your required format

Description

EcoPaXX® is our bio-based, high-performance polyamide (PA410) that offers outstanding performance across the board, while being made mainly from tropical castor beans which don’t compete with the food chain.
EcoPaXX® belongs to the family of long-chain polyamides, which offer exceptional performance in the most demanding of environments. That includes excellent chemical resistance, low moisture absorption, combined with a very high melting point (highest of all bio-plastics) and high crystallization rate (typical for engineering plastics like PA66 and PA46).
EcoPaXX® has the lowest carbon footprint amongst common polyamides. This is because the amount of carbon dioxide emitted during the production of EcoPaXX® is offset by the amount absorbed in plant growth, and in particular by the riccinus communis – the tropical castor bean plant that makes up some 70% of EcoPaXX®. Externally certified lifecycle analysis (LCA) data is available upon request.

Datasheet URL:

EcoPaXX® Q170E-H B-MB

Diese Materialdaten wurden von DSM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyValueConditionTesting Standard

Bio-based content

70 %

Show Supplier Material materials with Bio-based content of 70 %

dry

ASTM D6866-12 Method B

Dichte

1.09 g/cm³

Show Supplier Material materials with Dichte of 1.09 g/cm³

dry

ISO 1183

Moisture absorption

1.9 %

Show Supplier Material materials with Moisture absorption of 1.9 %

dry

Sim. to ISO 62

Wasserabsorption

5.8 %

Show Supplier Material materials with Wasserabsorption of 5.8 %

dry

Sim. to ISO 62

Mechanisch

PropertyTemperatureValueConditionTesting Standard

Dehnung

20 %

Show Supplier Material materials with Dehnung of 20 %

dry

ISO 527-1/-2

50 %

Show Supplier Material materials with Dehnung of 50 %

conditioned

ISO 527-1/-2

120 °C

200 %

Show Supplier Material materials with Dehnung of 200 %

dry

ISO 527-1/-2

140 °C

200 %

Show Supplier Material materials with Dehnung of 200 %

dry

ISO 527-1/-2

Elastizitätsmodul

1.6 GPa

Show Supplier Material materials with Elastizitätsmodul of 1.6 GPa

conditioned

ISO 527-1/-2

3.2 GPa

Show Supplier Material materials with Elastizitätsmodul of 3.2 GPa

dry

ISO 527-1/-2

120 °C

0.6 GPa

Show Supplier Material materials with Elastizitätsmodul of 0.6 GPa

dry

ISO 527-1/-2

140 °C

0.52 GPa

Show Supplier Material materials with Elastizitätsmodul of 0.52 GPa

dry

ISO 527-1/-2

Elongation at yield

4.6 %

Show Supplier Material materials with Elongation at yield of 4.6 %

dry

ISO 527-1/-2

20 %

Show Supplier Material materials with Elongation at yield of 20 %

conditioned

ISO 527-1/-2

Schlagfestigkeit, Charpy gekerbt

-30 °C

4 kJ/m²

Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m²

dry

ISO 179/1eA

-30 °C

4.5 kJ/m²

Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4.5 kJ/m²

conditioned

ISO 179/1eA

23 °C

5.5 kJ/m²

Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5.5 kJ/m²

dry

ISO 179/1eA

23 °C

12 kJ/m²

Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m²

conditioned

ISO 179/1eA

Zugfestigkeit

45 MPa

Show Supplier Material materials with Zugfestigkeit of 45 MPa

conditioned

ISO 527-1/-2

55.0 MPa

Show Supplier Material materials with Zugfestigkeit of 55.0 MPa

dry

ISO 527-1/-2

120 °C

38 MPa

Show Supplier Material materials with Zugfestigkeit of 38 MPa

dry

ISO 527-1/-2

140 °C

32 MPa

Show Supplier Material materials with Zugfestigkeit of 32 MPa

dry

ISO 527-1/-2

Thermisch

PropertyValueConditionTesting StandardPressureComment

Schmelzpunkt

250 °C

Show Supplier Material materials with Schmelzpunkt of 250 °C

dry

ISO 11357-1/-3

10°C/min

Wärmeformbeständigkeitstemperatur

75 °C

Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 75 °C

dry

ISO 75-1/-2

2 MPa

175 °C

Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 175 °C

dry

ISO 75-1/-2

0.45 MPa

Rheological Properties

PropertyTemperatureValueConditionTesting Standard

Schmelzmassenflussrate

280 °C

24 g/10min

Show Supplier Material materials with Schmelzmassenflussrate of 24 g/10min

dry

ISO 1133

Schmelzvolumenflussrate

280 °C

26 cm³/10min

Show Supplier Material materials with Schmelzvolumenflussrate of 26 cm³/10min

dry

ISO 1133

Viscosity number

170 cm³/gr

Show Supplier Material materials with Viscosity number of 170 cm³/gr

dry

ISO 307, 1157, 1628