Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.12 % Show Supplier Material materials with Moisture absorption of 0.12 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.3 % Show Supplier Material materials with Wasserabsorption of 0.3 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 17.5 GPa Show Supplier Material materials with Biegemodul of 17.5 GPa | dry | ISO 178 | |
Dehnung | 2 % Show Supplier Material materials with Dehnung of 2 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 19 GPa Show Supplier Material materials with Elastizitätsmodul of 19 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 330 MPa Show Supplier Material materials with Flexural yield strength of 330 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | dry | ISO 179/1eA |
23 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 55.0 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 55.0 kJ/m² | dry | ISO 179/1eU |
23 °C | 55.0 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 55.0 kJ/m² | dry | ISO 179/1eU | |
Zugfestigkeit | 210 MPa Show Supplier Material materials with Zugfestigkeit of 210 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
3.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | dry | UL746B | 0.81 mm | ||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | dry | UL746B | 0.81 mm | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | UL746B | 0.81 mm | ||
Schmelzpunkt | 255 °C Show Supplier Material materials with Schmelzpunkt of 255 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 240 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 240 °C | dry | ISO 75-1/-2 | 2 MPa | ||
252 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 252 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-] | dry | IEC 62631-2-1 | 1MHz |
3.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.8 [-] | dry | IEC 62631-2-1 | 100Hz | |
Kriechstromfestigkeit | 250 V Show Supplier Material materials with Kriechstromfestigkeit of 250 V | dry | IEC 60112 | |
Verlustfaktor | 20 [-] Show Supplier Material materials with Verlustfaktor of 20 [-] | dry | IEC 62631-2-1 | 100Hz |
110 [-] Show Supplier Material materials with Verlustfaktor of 110 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |