Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.36 g/cm³ Show Supplier Material materials with Dichte of 1.36 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 3.3 GPa Show Supplier Material materials with Biegemodul of 3.3 GPa | conditioned | ISO 178 | |
6.6 GPa Show Supplier Material materials with Biegemodul of 6.6 GPa | dry | ISO 178 | ||
Dehnung | 4 % Show Supplier Material materials with Dehnung of 4 % | dry | ISO 527-1/-2 | |
7 % Show Supplier Material materials with Dehnung of 7 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 4.2 GPa Show Supplier Material materials with Elastizitätsmodul of 4.2 GPa | conditioned | ISO 527-1/-2 | |
7.2 GPa Show Supplier Material materials with Elastizitätsmodul of 7.2 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | conditioned | ISO 178 | |
210 MPa Show Supplier Material materials with Flexural yield strength of 210 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA |
23 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 58.0 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 58.0 kJ/m² | dry | ISO 179/1eU |
23 °C | 75 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 75 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 75 MPa Show Supplier Material materials with Zugfestigkeit of 75 MPa | conditioned | ISO 527-1/-2 | |
135 MPa Show Supplier Material materials with Zugfestigkeit of 135 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 165 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 165 °C | dry | ISO 75-1/-2 | 2 MPa | |
210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 250 °C | 10 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 10 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 0.7 % Show Supplier Material materials with Schrumpfung of 0.7 % | dry | Sim. to ISO 294-4 | Parallel | |
0.8 % Show Supplier Material materials with Schrumpfung of 0.8 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |