Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.42 g/cm³ Show Supplier Material materials with Dichte of 1.42 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Wasserabsorption | 5.5 % Show Supplier Material materials with Wasserabsorption of 5.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 11.5 GPa Show Supplier Material materials with Biegemodul of 11.5 GPa | dry | ISO 178 | |
Dehnung | 1.8 % Show Supplier Material materials with Dehnung of 1.8 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 12 GPa Show Supplier Material materials with Elastizitätsmodul of 12 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 210 MPa Show Supplier Material materials with Flexural yield strength of 210 MPa | dry | ISO 178 | |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 4.5 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 4.5 kJ/m² | dry | ISO 179/1eU |
Zugfestigkeit | 150 MPa Show Supplier Material materials with Zugfestigkeit of 150 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 205 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 205 °C | dry | ISO 75-1/-2 | 2 MPa | |
215 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 500 Ω/sq Show Supplier Material materials with Surface resistivity of 500 Ω/sq | conditioned | IEC 62631-3-2 |
Technological properties
Property |
---|