Wrought Copper Bronze Aluminium Bronze
AMPCO® 18 Extruded and drawn rounds and rectangular barsGeliefert von:
AMPCO METALWrought Copper Bronze Aluminium Bronze
DEF STAN 02-833 / NES 833 BronzeWrought Copper Bronze Aluminium Bronze
BS CA104 / BSB23 / DTD197A BronzePhosphorbronze
EN 1652 Grade CuSn8 R450Phosphorbronze
EN 1652 Grade CuSn8 R540Phosphorbronze
EN 1652 Grade CuSn8 R600Phosphorbronze
EN 1652 Grade CuSn8 R660Phosphorbronze
EN 1652 Grade CuSn8 R740Phosphorbronze
EN 1652 Grade CuSn8 H135Phosphorbronze
EN 1652 Grade CuSn8 H170Phosphorbronze
EN 1652 Grade CuSn8 H190Phosphorbronze
EN 1652 Grade CuSn8 H210Phosphorbronze
EN 1652 Grade CuSn8 H230