Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.8 g/cm³ Show Supplier Material materials with Dichte of 10.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 15 % Show Supplier Material materials with Dehnung of 15 % | min. |
Elastizitätsmodul | 23.0 °C | 106 GPa Show Supplier Material materials with Elastizitätsmodul of 106 GPa | |
Härte, Vickers | 23.0 °C | 180 - 220 [-] Show Supplier Material materials with Härte, Vickers of 180 - 220 [-] | |
Zugfestigkeit | 23.0 °C | 580 - 680 MPa Show Supplier Material materials with Zugfestigkeit of 580 - 680 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 1070 - 1130 °C Show Supplier Material materials with Schmelzpunkt of 1070 - 1130 °C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 6.6 - 7 % IACS Show Supplier Material materials with Specific Electrical conductivity of 6.6 - 7 % IACS | |
Temperaturwiderstandskoeffizient | 23.0 °C | 3.9E-4 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of 3.9E-4 1/K |
spezifischer Widerstand | 23.0 °C | 2.45E-7 - 2.62E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.45E-7 - 2.62E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes, Potentiometers, battery contacts | |
Corrosion properties | Corrosion resistant | |
Other | Superb sliding contact alloy, stable contact resistance, wear resistant, oxidation resistant up to 300 °C, ductile, Age hardenable |