Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 11.8 g/cm³ Show Supplier Material materials with Dichte of 11.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 2 - 10 % Show Supplier Material materials with Dehnung of 2 - 10 % |
Elastizitätsmodul | 23.0 °C | 108 GPa Show Supplier Material materials with Elastizitätsmodul of 108 GPa |
Härte, Vickers | 23.0 °C | 260 - 340 [-] Show Supplier Material materials with Härte, Vickers of 260 - 340 [-] |
Schubmodule | 23.0 °C | 40 GPa Show Supplier Material materials with Schubmodule of 40 GPa |
Zugfestigkeit | 23.0 °C | 850 - 1150 MPa Show Supplier Material materials with Zugfestigkeit of 850 - 1150 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.46E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.46E-5 1/K | RT-100 °C |
Schmelzpunkt | 1130 - 1180 °C Show Supplier Material materials with Schmelzpunkt of 1130 - 1180 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 28 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 28 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 4.8 - 5.1 % IACS Show Supplier Material materials with Specific Electrical conductivity of 4.8 - 5.1 % IACS | |
Temperaturwiderstandskoeffizient | 23.0 °C | 2.8E-4 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of 2.8E-4 1/K |
spezifischer Widerstand | 23.0 °C | 3.38E-7 - 3.59E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3.38E-7 - 3.59E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes, Potentiometers, probe pins | |
Corrosion properties | Corrosion resistant | |
Other | Superb sliding contact alloy, stable contact resistance, wear resistant, Oxidation resistant up to 300 °C, Ductile |