Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 15.1 g/cm³ Show Supplier Material materials with Dichte of 15.1 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % | min. |
Elastizitätsmodul | 23.0 °C | 87 GPa Show Supplier Material materials with Elastizitätsmodul of 87 GPa | |
Härte, Vickers | 23.0 °C | 120 - 170 [-] Show Supplier Material materials with Härte, Vickers of 120 - 170 [-] | |
Schubmodule | 23.0 °C | 37 GPa Show Supplier Material materials with Schubmodule of 37 GPa | |
Zugfestigkeit | 23.0 °C | 400 - 600 MPa Show Supplier Material materials with Zugfestigkeit of 400 - 600 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.67E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.67E-5 1/K | RT-100 °C |
Schmelzpunkt | 865 - 895 °C Show Supplier Material materials with Schmelzpunkt of 865 - 895 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 66 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 66 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 11.9 - 13.8 % IACS Show Supplier Material materials with Specific Electrical conductivity of 11.9 - 13.8 % IACS | |
Temperaturwiderstandskoeffizient | 23.0 °C | 5.2E-4 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of 5.2E-4 1/K |
spezifischer Widerstand | 23.0 °C | 1.25E-7 - 1.45E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.25E-7 - 1.45E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes, Resistance wires | |
Corrosion properties | Corrosion resistant | |
Other | Wear resistant, Age hardenable, Ductile, High electrical conductivity, Stable Contact resistant |