Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.13 g/cm³ Show Supplier Material materials with Dichte of 10.13 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 20 % Show Supplier Material materials with Dehnung of 20 % | min. |
Elastizitätsmodul | 23.0 °C | 85 GPa Show Supplier Material materials with Elastizitätsmodul of 85 GPa | |
Härte, Vickers | 23.0 °C | 80 - 120 [-] Show Supplier Material materials with Härte, Vickers of 80 - 120 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 200 - 300 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 200 - 300 MPa | |
Zugfestigkeit | 23.0 °C | 300 - 400 MPa Show Supplier Material materials with Zugfestigkeit of 300 - 400 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.93E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.93E-5 1/K | RT-100 °C |
Schmelzpunkt | 779 - 820 °C Show Supplier Material materials with Schmelzpunkt of 779 - 820 °C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 70 - 77 % IACS Show Supplier Material materials with Specific Electrical conductivity of 70 - 77 % IACS | |
Temperaturwiderstandskoeffizient | 23.0 °C | 4.3E-4 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of 4.3E-4 1/K |
spezifischer Widerstand | 23.0 °C | 2.2E-8 - 2.5E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.2E-8 - 2.5E-8 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes, switching contacts | |
Corrosion properties | Corrosion resistant | |
Other | Ductile, High conductivity, Low contact resistance, Susceptible to attack by sulphur |