Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.4 g/cm³ Show Supplier Material materials with Dichte of 10.4 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 30 % Show Supplier Material materials with Dehnung of 30 % | min. |
Elastizitätsmodul | 23.0 °C | 76 GPa Show Supplier Material materials with Elastizitätsmodul of 76 GPa | |
Härte, Vickers | 23.0 °C | 30 - 80 [-] Show Supplier Material materials with Härte, Vickers of 30 - 80 [-] | |
Schubmodule | 23.0 °C | 24 GPa Show Supplier Material materials with Schubmodule of 24 GPa | |
Streckgrenze Rp 0,2 | 23.0 °C | 50 - 190 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 50 - 190 MPa | |
Zugfestigkeit | 23.0 °C | 170 - 260 MPa Show Supplier Material materials with Zugfestigkeit of 170 - 260 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.85E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.85E-5 1/K | RT-100 °C |
Schmelzpunkt | 900 - 938 °C Show Supplier Material materials with Schmelzpunkt of 900 - 938 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 372 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 372 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 90.5 - 95.6 % IACS Show Supplier Material materials with Specific Electrical conductivity of 90.5 - 95.6 % IACS | |
Temperaturwiderstandskoeffizient | 23.0 °C | 2.5E-3 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of 2.5E-3 1/K |
spezifischer Widerstand | 23.0 °C | 1.8E-8 - 1.9E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.8E-8 - 1.9E-8 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Collectors, communicators | |
Corrosion properties | Corrosion resistant | |
Other | Ductile, can be roll clad, formable, machinable, sensitive to sulphur |