Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 18.8 g/cm³ Show Supplier Material materials with Dichte of 18.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 1 - 2 % Show Supplier Material materials with Dehnung of 1 - 2 % |
Elastizitätsmodul | 23.0 °C | 180 GPa Show Supplier Material materials with Elastizitätsmodul of 180 GPa |
Härte, Vickers | 23.0 °C | 370 - 420 [-] Show Supplier Material materials with Härte, Vickers of 370 - 420 [-] |
Schubmodule | 23.0 °C | 74 GPa Show Supplier Material materials with Schubmodule of 74 GPa |
Streckgrenze Rp 0,2 | 23.0 °C | 1050 - 1200 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 1050 - 1200 MPa |
Zugfestigkeit | 23.0 °C | 1160 - 1230 MPa Show Supplier Material materials with Zugfestigkeit of 1160 - 1230 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.02E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.02E-5 1/K | RT-100 °C |
Schmelzpunkt | 1660 - 1700 °C Show Supplier Material materials with Schmelzpunkt of 1660 - 1700 °C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Specific Electrical conductivity | 5.6 - 5.77 % IACS Show Supplier Material materials with Specific Electrical conductivity of 5.6 - 5.77 % IACS | ||
Temperaturwiderstandskoeffizient | 23.0 °C | 1.25E-3 - 1.35E-3 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of 1.25E-3 - 1.35E-3 1/K | 0-100 °C |
spezifischer Widerstand | 23.0 °C | 2.98E-7 - 3.04E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.98E-7 - 3.04E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Spark plugs, electrodes | |
Corrosion properties | Corrosion resistant | |
Other | Ductile |