Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 20.73 g/cm³ Show Supplier Material materials with Dichte of 20.73 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 32.6 % Show Supplier Material materials with Dehnung of 32.6 % |
1200.0 °C | 57 % Show Supplier Material materials with Dehnung of 57 % | |
1400.0 °C | 63 % Show Supplier Material materials with Dehnung of 63 % | |
1600.0 °C | 55 % Show Supplier Material materials with Dehnung of 55 % | |
Elastizitätsmodul | 23.0 °C | 97.02 GPa Show Supplier Material materials with Elastizitätsmodul of 97.02 GPa |
Härte, Vickers | 23.0 °C | 73 [-] Show Supplier Material materials with Härte, Vickers of 73 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 114 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 114 MPa |
1200.0 °C | 27.1 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 27.1 MPa | |
1400.0 °C | 17.8 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 17.8 MPa | |
1600.0 °C | 10.1 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 10.1 MPa | |
Zugfestigkeit | 20.0 °C | 231 MPa Show Supplier Material materials with Zugfestigkeit of 231 MPa |
1200.0 °C | 44.2 MPa Show Supplier Material materials with Zugfestigkeit of 44.2 MPa | |
1400.0 °C | 25.3 MPa Show Supplier Material materials with Zugfestigkeit of 25.3 MPa | |
1600.0 °C | 13.2 MPa Show Supplier Material materials with Zugfestigkeit of 13.2 MPa | |
Thermisch
Property | Temperature | Value |
---|---|---|
Wärmeleitfähigkeit | 20.0 °C | 45.74 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 45.74 W/(m·K) |
1200.0 °C | 75.9 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 75.9 W/(m·K) | |
1400.0 °C | 77.16 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 77.16 W/(m·K) | |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 1.7E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.7E-7 Ω·m |
1146.0 °C | 5.2E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.2E-7 Ω·m | |