Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 20.59 g/cm³ Show Supplier Material materials with Dichte of 20.59 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 39 % Show Supplier Material materials with Dehnung of 39 % |
1200.0 °C | 59 % Show Supplier Material materials with Dehnung of 59 % | |
1400.0 °C | 68 % Show Supplier Material materials with Dehnung of 68 % | |
1600.0 °C | 71 % Show Supplier Material materials with Dehnung of 71 % | |
Elastizitätsmodul | 23.0 °C | 106 GPa Show Supplier Material materials with Elastizitätsmodul of 106 GPa |
Härte, Vickers | 23.0 °C | 82 [-] Show Supplier Material materials with Härte, Vickers of 82 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 128 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 128 MPa |
1200.0 °C | 40 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 40 MPa | |
1400.0 °C | 27 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 27 MPa | |
1600.0 °C | 16.1 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 16.1 MPa | |
Zugfestigkeit | 20.0 °C | 290 MPa Show Supplier Material materials with Zugfestigkeit of 290 MPa |
1200.0 °C | 55.3 MPa Show Supplier Material materials with Zugfestigkeit of 55.3 MPa | |
1400.0 °C | 31.2 MPa Show Supplier Material materials with Zugfestigkeit of 31.2 MPa | |
1600.0 °C | 19.2 MPa Show Supplier Material materials with Zugfestigkeit of 19.2 MPa | |
Thermisch
Property | Temperature | Value |
---|---|---|
Wärmeleitfähigkeit | 20.0 °C | 45.2 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 45.2 W/(m·K) |
1200.0 °C | 72.6 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 72.6 W/(m·K) | |
1400.0 °C | 74.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 74.7 W/(m·K) | |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 1.7E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.7E-7 Ω·m |
1146.0 °C | 5.3E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.3E-7 Ω·m | |
1369.0 °C | 6E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 6E-7 Ω·m | |