Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 19.87 g/cm³ Show Supplier Material materials with Dichte of 19.87 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 1200.0 °C | 28 % Show Supplier Material materials with Dehnung of 28 % | |
1400.0 °C | 32 % Show Supplier Material materials with Dehnung of 32 % | ||
1600.0 °C | 56 % Show Supplier Material materials with Dehnung of 56 % | ||
Elastizitätsmodul | 1200.0 °C | 142.2 GPa Show Supplier Material materials with Elastizitätsmodul of 142.2 GPa | |
Härte, Vickers | 23.0 °C | 130 [-] Show Supplier Material materials with Härte, Vickers of 130 [-] | |
Kriechfestigkeit | 1200.0 °C | 7.6 MPa Show Supplier Material materials with Kriechfestigkeit of 7.6 MPa | 10,000 h (extrapolated data) |
1400.0 °C | 6.8 MPa Show Supplier Material materials with Kriechfestigkeit of 6.8 MPa | 10,000 h (extrapolated data) | |
1600.0 °C | 4.6 MPa Show Supplier Material materials with Kriechfestigkeit of 4.6 MPa | 10,000 h (extrapolated data) | |
Norton Exponent | 1200.0 °C | 6.7 [-] Show Supplier Material materials with Norton Exponent of 6.7 [-] | |
1400.0 °C | 11.6 [-] Show Supplier Material materials with Norton Exponent of 11.6 [-] | ||
1600.0 °C | 11 [-] Show Supplier Material materials with Norton Exponent of 11 [-] | ||
Streckgrenze Rp 0,2 | 1200.0 °C | 57 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 57 MPa | |
1400.0 °C | 40 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 40 MPa | ||
1600.0 °C | 27 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 27 MPa | ||
Zugfestigkeit | 1200.0 °C | 85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | |
1400.0 °C | 52 MPa Show Supplier Material materials with Zugfestigkeit of 52 MPa | ||
1600.0 °C | 31 MPa Show Supplier Material materials with Zugfestigkeit of 31 MPa | ||
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 1840 - 1870 °C Show Supplier Material materials with Schmelzpunkt of 1840 - 1870 °C | |
Wärmeleitfähigkeit | 20.0 °C | 40.3 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 40.3 W/(m·K) |
1200.0 °C | 66.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 66.7 W/(m·K) | |
1400.0 °C | 69.5 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 69.5 W/(m·K) | |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 1.5E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.5E-7 Ω·m |
1156.0 °C | 5.5E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.5E-7 Ω·m | |
1400.0 °C | 6.1E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 6.1E-7 Ω·m | |