Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-80 mm - Sheet: 40x20-40x25 mm |
Mechanisch
Property | Value |
---|---|
Zugfestigkeit | 800.0 - 950.0 MPa Show Supplier Material materials with Zugfestigkeit of 800.0 - 950.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15.0 - 18.0 % Show Supplier Material materials with Chrom of 15.0 - 18.0 % | |
Kohlenstoff | 0.12 - 0.2 % Show Supplier Material materials with Kohlenstoff of 0.12 - 0.2 % | |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. |
Nickel | 2.0 - 3.0 % Show Supplier Material materials with Nickel of 2.0 - 3.0 % | |
Phosphor | 0.035 % Show Supplier Material materials with Phosphor of 0.035 % | max. |
Schwefel | 0.025 % Show Supplier Material materials with Schwefel of 0.025 % | max. |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Chemical industry, Nuclear plants | |
Processing history | Quenched and Tempered |