Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-210 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 30 % Show Supplier Material materials with Dehnung of 30 % | min. |
Härte, Brinell | 215 [-] Show Supplier Material materials with Härte, Brinell of 215 [-] | max. |
Streckgrenze | 170.0 MPa Show Supplier Material materials with Streckgrenze of 170.0 MPa | min., RP02 |
Zugfestigkeit | 500.0 - 700.0 MPa Show Supplier Material materials with Zugfestigkeit of 500.0 - 700.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 16.5 - 18.5 % Show Supplier Material materials with Chrom of 16.5 - 18.5 % | |
Kohlenstoff | 0.05 % Show Supplier Material materials with Kohlenstoff of 0.05 % | max. |
Mangan | 2.0 % Show Supplier Material materials with Mangan of 2.0 % | max. |
Molybdän | 2.5 - 3.0 % Show Supplier Material materials with Molybdän of 2.5 - 3.0 % | |
Nickel | 10.5 - 13.0 % Show Supplier Material materials with Nickel of 10.5 - 13.0 % | |
Phosphor | 0.045 % Show Supplier Material materials with Phosphor of 0.045 % | max. |
Schwefel | 0.02 % Show Supplier Material materials with Schwefel of 0.02 % | max. |
Silizium | 1.0 % Show Supplier Material materials with Silizium of 1.0 % | max. |
Stickstoff | 0.11 % Show Supplier Material materials with Stickstoff of 0.11 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant engineering, petrochemistry, apparatus engineering, shipbuilding, chemistry, power plant construction, vehicle construction, aerospace, food technology, pharmacy, agricultural engineering | |
Processing history | Solution Annealed |