Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-70 mm - Hexagonal Bar: 13- 50 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 25 % Show Supplier Material materials with Dehnung of 25 % | min. |
Härte, Brinell | 270 [-] Show Supplier Material materials with Härte, Brinell of 270 [-] | max. |
Streckgrenze | 450.0 MPa Show Supplier Material materials with Streckgrenze of 450.0 MPa | min., RP02 |
Zugfestigkeit | 650.0 - 880.0 MPa Show Supplier Material materials with Zugfestigkeit of 650.0 - 880.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 21.0 - 23.0 % Show Supplier Material materials with Chrom of 21.0 - 23.0 % | |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | max. |
Mangan | 2.0 % Show Supplier Material materials with Mangan of 2.0 % | max. |
Molybdän | 2.5 - 3.01 % Show Supplier Material materials with Molybdän of 2.5 - 3.01 % | |
Nickel | 4.5 - 6.5 % Show Supplier Material materials with Nickel of 4.5 - 6.5 % | |
Phosphor | 0.035 % Show Supplier Material materials with Phosphor of 0.035 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1.0 % Show Supplier Material materials with Silizium of 1.0 % | max. |
Stickstoff | 0.1 - 0.22 % Show Supplier Material materials with Stickstoff of 0.1 - 0.22 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, petrochemistry, shipbuilding, apparatus engineering, chemistry, power plant construction, aerospace, offshore, power generation, rail vehicles, electrical engineering, mechanical engineering | |
Processing history | Solution Annealed and blank |