Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-149.23 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 45 % Show Supplier Material materials with Dehnung of 45 % | min. |
Streckgrenze | 1150.0 MPa Show Supplier Material materials with Streckgrenze of 1150.0 MPa | min., RP02 |
Zugfestigkeit | 1220.0 - 1400.0 MPa Show Supplier Material materials with Zugfestigkeit of 1220.0 - 1400.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.8 - 1.35 % Show Supplier Material materials with Aluminium of 0.8 - 1.35 % | |
Chrom | 12.25 - 13.25 % Show Supplier Material materials with Chrom of 12.25 - 13.25 % | |
Kohlenstoff | 0.05 % Show Supplier Material materials with Kohlenstoff of 0.05 % | max. |
Mangan | 0.1 % Show Supplier Material materials with Mangan of 0.1 % | max. |
Molybdän | 2.0 - 2.5 % Show Supplier Material materials with Molybdän of 2.0 - 2.5 % | |
Nickel | 7.5 - 8.5 % Show Supplier Material materials with Nickel of 7.5 - 8.5 % | |
Phosphor | 0.01 % Show Supplier Material materials with Phosphor of 0.01 % | max. |
Schwefel | 0.008 % Show Supplier Material materials with Schwefel of 0.008 % | max. |
Silizium | 0.1 % Show Supplier Material materials with Silizium of 0.1 % | max. |
Stickstoff | 0.01 % Show Supplier Material materials with Stickstoff of 0.01 % | max. |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Vehicle construction, connecting parts, aerospace, mechanical engineering | |
Processing history | Hardened |