Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-230 mm partly ESU - Sheet: 17x15-241x63.5 - Rectangular Bar: 51 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Zugfestigkeit | 1200 MPa Show Supplier Material materials with Zugfestigkeit of 1200 MPa | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15.0 - 17.0 % Show Supplier Material materials with Chrom of 15.0 - 17.0 % | |
Kohlenstoff | 0.07 % Show Supplier Material materials with Kohlenstoff of 0.07 % | max. |
Kupfer | 3.0 - 5.0 % Show Supplier Material materials with Kupfer of 3.0 - 5.0 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Molybdän | 0.6 % Show Supplier Material materials with Molybdän of 0.6 % | max. |
Nickel | 3.0 - 5.0 % Show Supplier Material materials with Nickel of 3.0 - 5.0 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.7 % Show Supplier Material materials with Silizium of 0.7 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, mechanical engineering, medical technology, aerospace, screws and spindle material in valve construction, wheel and cover discs in compressor construction | |
Processing history | Solution Annealed |