Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-370 mm partly ESU |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 16 % Show Supplier Material materials with Dehnung of 16 % | min. |
Härte, Brinell | 311 [-] Show Supplier Material materials with Härte, Brinell of 311 [-] | min. |
Streckgrenze | 725.0 MPa Show Supplier Material materials with Streckgrenze of 725.0 MPa | min., RP02 |
Zugfestigkeit | 860 MPa Show Supplier Material materials with Zugfestigkeit of 860 MPa | min. |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15.0 - 17.0 % Show Supplier Material materials with Chrom of 15.0 - 17.0 % | |
Kohlenstoff | 0.07 % Show Supplier Material materials with Kohlenstoff of 0.07 % | max. |
Kupfer | 3.0 - 5.0 % Show Supplier Material materials with Kupfer of 3.0 - 5.0 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Molybdän | 0.6 % Show Supplier Material materials with Molybdän of 0.6 % | max. |
Nickel | 3.0 - 5.0 % Show Supplier Material materials with Nickel of 3.0 - 5.0 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.7 % Show Supplier Material materials with Silizium of 0.7 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, mechanical engineering, medical technology, aerospace, screws and spindle material in valve construction, wheel and cover discs in compressor construction | |
Processing history | Hardened |