Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-80 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 30 % Show Supplier Material materials with Dehnung of 30 % | min. |
Härte, Brinell | 140.0 - 215.0 [-] Show Supplier Material materials with Härte, Brinell of 140.0 - 215.0 [-] | |
Streckgrenze | 207.0 MPa Show Supplier Material materials with Streckgrenze of 207.0 MPa | min., RP02 |
Zugfestigkeit | 500.0 - 750.0 MPa Show Supplier Material materials with Zugfestigkeit of 500.0 - 750.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15.0 - 17.0 % Show Supplier Material materials with Chrom of 15.0 - 17.0 % | |
Kohlenstoff | 0.07 % Show Supplier Material materials with Kohlenstoff of 0.07 % | max. |
Kupfer | 3.0 - 5.0 % Show Supplier Material materials with Kupfer of 3.0 - 5.0 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Molybdän | 0.6 % Show Supplier Material materials with Molybdän of 0.6 % | max. |
Nickel | 3.0 - 5.0 % Show Supplier Material materials with Nickel of 3.0 - 5.0 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.7 % Show Supplier Material materials with Silizium of 0.7 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace | |
Processing history | Solution Annealed |