Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-230 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 17.0 - 19.0 % Show Supplier Material materials with Chrom of 17.0 - 19.0 % | |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | max. |
Mangan | 2.0 % Show Supplier Material materials with Mangan of 2.0 % | max. |
Nickel | 10.0 - 12.0 % Show Supplier Material materials with Nickel of 10.0 - 12.0 % | |
Phosphor | 0.035 % Show Supplier Material materials with Phosphor of 0.035 % | max. |
Schwefel | 0.025 % Show Supplier Material materials with Schwefel of 0.025 % | max. |
Silizium | 1.0 % Show Supplier Material materials with Silizium of 1.0 % | max. |
Titan | 0.7 % Show Supplier Material materials with Titan of 0.7 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace | |
Processing history | Solution Annealed |