Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-240 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 8 % Show Supplier Material materials with Dehnung of 8 % | min. |
Härte, Brinell | 331.0 - 392.0 [-] Show Supplier Material materials with Härte, Brinell of 331.0 - 392.0 [-] | |
Streckgrenze | 1000.0 MPa Show Supplier Material materials with Streckgrenze of 1000.0 MPa | min., RP02 |
Zugfestigkeit | 1070 MPa Show Supplier Material materials with Zugfestigkeit of 1070 MPa | min. |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15.0 - 15.5 % Show Supplier Material materials with Chrom of 15.0 - 15.5 % | |
Kohlenstoff | 0.07 % Show Supplier Material materials with Kohlenstoff of 0.07 % | max. |
Kupfer | 2.5 - 4.5 % Show Supplier Material materials with Kupfer of 2.5 - 4.5 % | |
Mangan | 1.0 % Show Supplier Material materials with Mangan of 1.0 % | max. |
Molybdän | 0.5 % Show Supplier Material materials with Molybdän of 0.5 % | max. |
Nickel | 3.0 - 5.5 % Show Supplier Material materials with Nickel of 3.0 - 5.5 % | |
Niobium | 0.005 % Show Supplier Material materials with Niobium of 0.005 % | max. |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1.0 % Show Supplier Material materials with Silizium of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace | |
Processing history | Hardened |