Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-240 mm - Sheet: 17x15-254x63.5 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 7 % Show Supplier Material materials with Dehnung of 7 % | min. |
Streckgrenze | 1000.0 MPa Show Supplier Material materials with Streckgrenze of 1000.0 MPa | min., RP02 |
Zugfestigkeit | 1070 MPa Show Supplier Material materials with Zugfestigkeit of 1070 MPa | min. |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 17.0 - 19.0 % Show Supplier Material materials with Chrom of 17.0 - 19.0 % | |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | max. |
Kupfer | 0.03 % Show Supplier Material materials with Kupfer of 0.03 % | max. |
Mangan | 2.0 % Show Supplier Material materials with Mangan of 2.0 % | max. |
Nickel | 9.0 - 12.0 % Show Supplier Material materials with Nickel of 9.0 - 12.0 % | |
Niobium | 1.0 % Show Supplier Material materials with Niobium of 1.0 % | max. |
Phosphor | 0.045 % Show Supplier Material materials with Phosphor of 0.045 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1.0 % Show Supplier Material materials with Silizium of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace | |
Processing history | Hardened |