Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 10.5-95 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 1.4 - 1.7 % Show Supplier Material materials with Chrom of 1.4 - 1.7 % | |
Kohlenstoff | 0.14 - 0.19 % Show Supplier Material materials with Kohlenstoff of 0.14 - 0.19 % | |
Mangan | 0.4 - 0.6 % Show Supplier Material materials with Mangan of 0.4 - 0.6 % | |
Molybdän | 5 % Show Supplier Material materials with Molybdän of 5 % | max. |
Nickel | 1.4 - 1.7 % Show Supplier Material materials with Nickel of 1.4 - 1.7 % | |
Phosphor | 0.035 % Show Supplier Material materials with Phosphor of 0.035 % | max. |
Schwefel | 0.035 % Show Supplier Material materials with Schwefel of 0.035 % | max. |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Mechanical Engineering, Apparatus engineering | |
Processing history | Solution Annealed |