Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 32 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.015 - 0.08 % Show Supplier Material materials with Aluminium of 0.015 - 0.08 % | |
Arsen | 0.15 % Show Supplier Material materials with Arsen of 0.15 % | max. |
Bor | 0.001 - 0.01 % Show Supplier Material materials with Bor of 0.001 - 0.01 % | |
Chrom | 0.9 - 1.2 % Show Supplier Material materials with Chrom of 0.9 - 1.2 % | |
Kohlenstoff | 0.17 - 0.23 % Show Supplier Material materials with Kohlenstoff of 0.17 - 0.23 % | |
Kupfer | 0.2 % Show Supplier Material materials with Kupfer of 0.2 % | max. |
Mangan | 0.35 - 0.75 % Show Supplier Material materials with Mangan of 0.35 - 0.75 % | |
Molybdän | 0.9 - 1.1 % Show Supplier Material materials with Molybdän of 0.9 - 1.1 % | |
Nickel | 0.2 % Show Supplier Material materials with Nickel of 0.2 % | max. |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. |
Schwefel | 002 % Show Supplier Material materials with Schwefel of 002 % | max. |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | max. |
Titan | 0.07 - 0.15 % Show Supplier Material materials with Titan of 0.07 - 0.15 % | |
Vanadium | 0.6 - 0.8 % Show Supplier Material materials with Vanadium of 0.6 - 0.8 % | |
Zinn | 0.02 % Show Supplier Material materials with Zinn of 0.02 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Defense Technology | |
Processing history | Quenched and Tempered |