Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 14-120 mm - Sheet: 135x54-207x 54 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 0.25 - 1.5 % Show Supplier Material materials with Chrom of 0.25 - 1.5 % | |
Kohlenstoff | 0.12 - 0.18 % Show Supplier Material materials with Kohlenstoff of 0.12 - 0.18 % | |
Mangan | 0.8 - 1.0 % Show Supplier Material materials with Mangan of 0.8 - 1.0 % | |
Molybdän | 0.8 - 1.0 % Show Supplier Material materials with Molybdän of 0.8 - 1.0 % | |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.2 % Show Supplier Material materials with Silizium of 0.2 % | max. |
Vanadium | 0.2 - 0.3 % Show Supplier Material materials with Vanadium of 0.2 - 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Defense Technology | |
Processing history | Quenched and Tempered |