Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 40-210 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 18 % Show Supplier Material materials with Dehnung of 18 % | min. |
Streckgrenze | 420.0 MPa Show Supplier Material materials with Streckgrenze of 420.0 MPa | min., RP02 |
Zugfestigkeit | 600.0 - 1100.0 MPa Show Supplier Material materials with Zugfestigkeit of 600.0 - 1100.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 0.9 - 1.2 % Show Supplier Material materials with Chrom of 0.9 - 1.2 % | |
Kohlenstoff | 0.22 - 0.29 % Show Supplier Material materials with Kohlenstoff of 0.22 - 0.29 % | |
Mangan | 0.5 - 0.8 % Show Supplier Material materials with Mangan of 0.5 - 0.8 % | |
Molybdän | 0.15 - 0.3 % Show Supplier Material materials with Molybdän of 0.15 - 0.3 % | |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.025 % Show Supplier Material materials with Schwefel of 0.025 % | |
Silizium | 0.35 % Show Supplier Material materials with Silizium of 0.35 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Tool technology, Automotive engineering, Aerospace | |
Processing history | Quenched and Tempered and Forged |