Acero inoxidable austenítico
Alloy 24 / 1.4565 Solution annealed and quenchedSuministrada por:
Hempel Special MetalsAcero inoxidable austenítico
Sandvik 2RE10Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
EN 10088-1 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Acero inoxidable austenítico
Sandvik 7RE10Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable dúplex
S32550 / AMAZON 256 Duplex Stainless SteelAcero inoxidable dúplex
S32760 / SEACOL-760 Duplex Stainless SteelAcero inoxidable austenítico
EN 10088-1 Grade X1CrNi25-21 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X1CrNiMoCuN25-25-5 solution annealed (+AT)Acero inoxidable dúplex
EN 10088-1 Grade X2CrNiN23-4 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X1CrNi25-21 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Acero inoxidable dúplex
EN 10028-7 Grade X2CrNiMoCuN25-6-3 solution annealed (+AT)Acero inoxidable dúplex
EN 10028-7 Grade X2CrNiMoCuWN25-7-4 solution annealed (+AT)Acero inoxidable dúplex
EN 10028-7 Grade X2CrNiMoN25-7-4 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X1CrNi25-21 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X1CrNiMoN25-22-2 solution annealed (+AT)