Coeficiente de dilatación térmica: 1.69E-5 - 1.72E-5 1/K

Quick Comparison

Polyamide 66 (PA66)

Zytel® 70G35HSL NC010

Polyamide 66 (PA66)

Zytel® 70G35HSLX BK357

Acero inoxidable austenítico

Sandvik 253 MA

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Wrought Copper Nickel Grade

UNS C70260 boway

Suministrada por:

Ningbo Boway Alloy Material

Polyamide 66 (PA66)

Zytel® 70G35EF NC010

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Nickel Chromium Iron Alloy

Sanicro® 28

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Wrought Copper High Copper Alloy

UNS C19210 boway

Suministrada por:

Ningbo Boway Alloy Material

Polyamide 66 (PA66)

Zytel® 70G35EF BK538

Tereftalato de polibutileno (PBT)

LNP™ THERMOTUF™ Compound WF008N

Suministrada por:

Sabic

Compuesto de matriz de polímero termoendurecible

Phenolic NP660 - Sheet

Suministrada por:

Norplex-Micarta

Acero inoxidable austenítico

Alloy 24 / 1.4565 Solution annealed and quenched

Suministrada por:

Hempel Special Metals

Polyamide 66 (PA66)

Zytel® 70G35HSRX BK099

Polyamide 66 (PA66)

Zytel® FR95G25V0NH BK458

Polyamide 66 (PA66)

Zytel® FR95G25V0NH NC010

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TF00

Nickel Chromium Iron Alloy

VDM® Alloy 718

Suministrada por:

VDM Metals

Polyamide 66 (PA66)

Zytel® 70G35HSL BK039B

Other Polyamide (PA)

Zytel® HTN53G50HSLR NC010
Página 1 de 393