Módulo elástico: 3.5 - 3.9 GPa

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3120-10

Suministrada por:

Arkema: High Performance Polymers

Polyamide 6 (PA6)

Akulon® F223-D

Suministrada por:

DSM Engineering Materials

Tereftalato de polibutileno (PBT)

Arnite® TV4 260 S

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K222-D

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K225-KS

Suministrada por:

DSM Engineering Materials

Polyvinylidenefluoride (PVDF)

Kynar® 370

Suministrada por:

Arkema: High Performance Polymers

Polyamide 66 (PA66)

Zytel® 135F NC010

Polyamide 6 (PA6)

Akulon® K223-KMV6

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-HG6

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® S223-HG6

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® F-X9190

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-HG3

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-G3

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-PG6

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® S223-HG7

Suministrada por:

DSM Engineering Materials

Policarbonato (PC)

LEXAN™ Copolymer EXL5689 - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer EXL5689 - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer EXL5689 - Europe

Suministrada por:

Sabic
Página 1 de 13