General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.32 g/cm³ Show Supplier Material materials with Density of 1.32 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Water absorption | 5.7 % Show Supplier Material materials with Water absorption of 5.7 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 4.8 GPa Show Supplier Material materials with Elastic modulus of 4.8 GPa | conditioned | ISO 527-1/-2 | |
8.7 GPa Show Supplier Material materials with Elastic modulus of 8.7 GPa | dry | ISO 527-1/-2 | ||
40 °C | 8.9 GPa Show Supplier Material materials with Elastic modulus of 8.9 GPa | dry | ISO 527-1/-2 | |
100 °C | 3.7 GPa Show Supplier Material materials with Elastic modulus of 3.7 GPa | dry | ISO 527-1/-2 | |
120 °C | 3.5 GPa Show Supplier Material materials with Elastic modulus of 3.5 GPa | dry | ISO 527-1/-2 | |
150 °C | 3.1 GPa Show Supplier Material materials with Elastic modulus of 3.1 GPa | dry | ISO 527-1/-2 | |
160 °C | 3.0 GPa Show Supplier Material materials with Elastic modulus of 3.0 GPa | dry | ISO 527-1/-2 | |
Elongation | -40 °C | 5 % Show Supplier Material materials with Elongation of 5 % | dry | ISO 527-1/-2 |
5 % Show Supplier Material materials with Elongation of 5 % | dry | ISO 527-1/-2 | ||
10 % Show Supplier Material materials with Elongation of 10 % | conditioned | ISO 527-1/-2 | ||
120 °C | 14.3 % Show Supplier Material materials with Elongation of 14.3 % | dry | ISO 527-1/-2 | |
150 °C | 15.2 % Show Supplier Material materials with Elongation of 15.2 % | dry | ISO 527-1/-2 | |
160 °C | 15.5 % Show Supplier Material materials with Elongation of 15.5 % | dry | ISO 527-1/-2 | |
Flexural modulus | 4.9 GPa Show Supplier Material materials with Flexural modulus of 4.9 GPa | conditioned | ISO 178 | |
8.5 GPa Show Supplier Material materials with Flexural modulus of 8.5 GPa | dry | ISO 178 | ||
Flexural yield strength | 140 MPa Show Supplier Material materials with Flexural yield strength of 140 MPa | conditioned | ISO 178 | |
250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | -30 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 23 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 23 kJ/m² | dry | ISO 179/1eA | |
23 °C | 43 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 43 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 95 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 95 kJ/m² | dry | ISO 179/1eU | |
23 °C | 110 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 110 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | -40 °C | 235 MPa Show Supplier Material materials with Tensile strength of 235 MPa | dry | ISO 527-1/-2 |
105 MPa Show Supplier Material materials with Tensile strength of 105 MPa | conditioned | ISO 527-1/-2 | ||
150 MPa Show Supplier Material materials with Tensile strength of 150 MPa | dry | ISO 527-1/-2 | ||
100 °C | 85 MPa Show Supplier Material materials with Tensile strength of 85 MPa | dry | ISO 527-1/-2 | |
120 °C | 80 MPa Show Supplier Material materials with Tensile strength of 80 MPa | dry | ISO 527-1/-2 | |
150 °C | 70 MPa Show Supplier Material materials with Tensile strength of 70 MPa | dry | ISO 527-1/-2 | |
160 °C | 65 MPa Show Supplier Material materials with Tensile strength of 65 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Thickness | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
9e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Heat deflection temperature | 200 °C Show Supplier Material materials with Heat deflection temperature of 200 °C | dry | ISO 75-1/-2 | 2 MPa | ||
215 °C Show Supplier Material materials with Heat deflection temperature of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Thermal diffusivity | 8.99e-08 mm²/s Show Supplier Material materials with Thermal diffusivity of 8.99e-08 mm²/s | dry | - |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | conditioned | IEC 60112 | |
Dielectric constant | 3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 62631-2-1 | 1MHz |
3.8 [-] Show Supplier Material materials with Dielectric constant of 3.8 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.5 [-] Show Supplier Material materials with Dielectric constant of 4.5 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
14.0 [-] Show Supplier Material materials with Dielectric constant of 14.0 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 20 kV/mm Show Supplier Material materials with Dielectric strength of 20 kV/mm | conditioned | IEC 60243-1 | |
25 kV/mm Show Supplier Material materials with Dielectric strength of 25 kV/mm | dry | IEC 60243-1 | ||
Dissipation factor | 90 [-] Show Supplier Material materials with Dissipation factor of 90 [-] | dry | IEC 62631-2-1 | 100Hz |
150 [-] Show Supplier Material materials with Dissipation factor of 150 [-] | dry | IEC 62631-2-1 | 1MHz | |
1200 [-] Show Supplier Material materials with Dissipation factor of 1200 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Dissipation factor of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 1110 g/cm³ Show Supplier Material materials with Density of melt of 1110 g/cm³ | dry | - | ||
Melt mass-flow rate | 24 g/10min Show Supplier Material materials with Melt mass-flow rate of 24 g/10min | dry | ISO 1133 | ||
Melt volume-flow rate | 275 °C | 20 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 20 cm³/10min | dry | ISO 1133 | |
Shrinkage | 0.39 % Show Supplier Material materials with Shrinkage of 0.39 % | dry | ISO 294-4 | Parallel | |
1 % Show Supplier Material materials with Shrinkage of 1 % | dry | ISO 294-4 | Normal | ||
Specific heat capacity melt | 2830.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2830.0 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.28 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.28 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Chainsaw housings, Powertool Housings, Skibinding Fixations, Inline Skate Frames, Airbag Containers | |
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |