Módulo elástico: 7.5 - 9 GPa

Quick Comparison

Polyamide 46 (PA46)

Stanyl® TE250F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TS250F6D

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® 46SF5030

Suministrada por:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® F11

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW250F6

Suministrada por:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® T11

Suministrada por:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® TX1

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW200F8

Suministrada por:

DSM Engineering Materials

Mezcla de polímeros

LNP™ THERMOCOMP™ Compound 6F006I

Suministrada por:

Sabic

Polyamide 46 (PA46)

Stanyl® TW241F10

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 70G25HSL NC010

Polyamide 66 (PA66)

Zytel® 80G33HS1L NC010

Polyamide 46 (PA46)

Stanyl® TE250F3

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F8

Suministrada por:

DSM Engineering Materials

Tereftalato de polibutileno (PBT)

VALOX™ FR Resins 4521

Polyamide 46 (PA46)

Stanyl® HFX61S

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 70G25HSLR NC010

Polyamide 66 (PA66)

Minlon® 22C NC010

Polyamide 6 (PA6)

Akulon® K224-HG8

Suministrada por:

DSM Engineering Materials
Página 1 de 20