General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density | 1.67 g/cm³ Show Supplier Material materials with Density of 1.67 g/cm³ | dry | ISO 1183 | |
Limiting oxygen index | 37 % Show Supplier Material materials with Limiting oxygen index of 37 % | dry | ISO 4589-1/-2 | |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 | |
Water absorption | 1.7 % Show Supplier Material materials with Water absorption of 1.7 % | dry | ISO 62 | at 23°C after 24h |
5.9 % Show Supplier Material materials with Water absorption of 5.9 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 8 GPa Show Supplier Material materials with Elastic modulus of 8 GPa | conditioned | ISO 527-1/-2 | |||
8 GPa Show Supplier Material materials with Elastic modulus of 8 GPa | conditioned | ISO 527-1/-2 | ||||
12 GPa Show Supplier Material materials with Elastic modulus of 12 GPa | dry | ISO 527-1/-2 | ||||
12 GPa Show Supplier Material materials with Elastic modulus of 12 GPa | dry | ISO 527-1/-2 | 1 mm | |||
120 °C | 7.5 GPa Show Supplier Material materials with Elastic modulus of 7.5 GPa | dry | ISO 527-1/-2 | |||
160 °C | 6.2 GPa Show Supplier Material materials with Elastic modulus of 6.2 GPa | dry | ISO 527-1/-2 | |||
Elongation | 2.4 % Show Supplier Material materials with Elongation of 2.4 % | dry | ISO 527-1/-2 | 1 mm | ||
2.5 % Show Supplier Material materials with Elongation of 2.5 % | dry | ISO 527-1/-2 | ||||
3.5 % Show Supplier Material materials with Elongation of 3.5 % | conditioned | ISO 527-1/-2 | ||||
3.8 % Show Supplier Material materials with Elongation of 3.8 % | conditioned | ISO 527-1/-2 | ||||
120 °C | 4 % Show Supplier Material materials with Elongation of 4 % | dry | ISO 527-1/-2 | |||
160 °C | 4 % Show Supplier Material materials with Elongation of 4 % | dry | ISO 527-1/-2 | |||
Flexural modulus | 7.3 GPa Show Supplier Material materials with Flexural modulus of 7.3 GPa | conditioned | ISO 178 | |||
11 GPa Show Supplier Material materials with Flexural modulus of 11 GPa | dry | ISO 178 | ||||
120 °C | 6.5 GPa Show Supplier Material materials with Flexural modulus of 6.5 GPa | dry | ISO 178 | |||
160 °C | 5 GPa Show Supplier Material materials with Flexural modulus of 5 GPa | dry | ISO 178 | |||
Flexural yield strength | 190 MPa Show Supplier Material materials with Flexural yield strength of 190 MPa | conditioned | ISO 178 | |||
260 MPa Show Supplier Material materials with Flexural yield strength of 260 MPa | dry | ISO 178 | ||||
120 °C | 170 MPa Show Supplier Material materials with Flexural yield strength of 170 MPa | dry | ISO 178 | |||
160 °C | 140 MPa Show Supplier Material materials with Flexural yield strength of 140 MPa | dry | ISO 178 | |||
Impact strength, Charpy notched | -30 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | dry, conditioned | ISO 179/1eA | ||
23 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m² | dry, conditioned | ISO 179/1eA | |||
Impact strength, Charpy unnotched | -30 °C | 50 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 50 kJ/m² | dry, conditioned | ISO 179/1eU | ||
23 °C | 60 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 60 kJ/m² | dry, conditioned | ISO 179/1eU | |||
Tensile strength | 120 MPa Show Supplier Material materials with Tensile strength of 120 MPa | conditioned | ISO 527-1/-2 | |||
120 MPa Show Supplier Material materials with Tensile strength of 120 MPa | conditioned | ISO 527-1/-2 | at low thickness | |||
180 MPa Show Supplier Material materials with Tensile strength of 180 MPa | dry | ISO 527-1/-2 | ||||
180 MPa Show Supplier Material materials with Tensile strength of 180 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness | ||
120 °C | 105 MPa Show Supplier Material materials with Tensile strength of 105 MPa | dry | ISO 527-1/-2 | |||
160 °C | 95 MPa Show Supplier Material materials with Tensile strength of 95 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 270 °C Show Supplier Material materials with Ball pressure temperature of 270 °C | dry | IEC 60695-10-2 | |||
Coefficient of thermal expansion | 2.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
5.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Glass transition temperature | 75 °C Show Supplier Material materials with Glass transition temperature of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | |||
Glow Wire Ignition Temperature | 825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | IEC 60695-2-13 | 0.75 mm | ||
850 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C | dry | IEC 60695-2-13 | 3 mm | |||
Heat deflection temperature | 290 °C Show Supplier Material materials with Heat deflection temperature of 290 °C | dry | ISO 75-1/-2 | 2 MPa | ||
290 °C Show Supplier Material materials with Heat deflection temperature of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 295 °C Show Supplier Material materials with Melting point of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 120 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120 °C | dry | UL746B | 0.75 mm | ||
Thermal diffusivity | 1.59e-07 mm²/s Show Supplier Material materials with Thermal diffusivity of 1.59e-07 mm²/s | dry | - | |||
Vicat softening temperature | 290 °C Show Supplier Material materials with Vicat softening temperature of 290 °C | dry | ISO 306 | 50°C/h 50N |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 225 V Show Supplier Material materials with Comparative tracking index of 225 V | dry | IEC 60112 | |
Dielectric constant | 3.6 [-] Show Supplier Material materials with Dielectric constant of 3.6 [-] | dry | IEC 60250 | 1GHz |
3.8 [-] Show Supplier Material materials with Dielectric constant of 3.8 [-] | conditioned | IEC 60250 | 1GHz | |
4 [-] Show Supplier Material materials with Dielectric constant of 4 [-] | dry | IEC 62631-2-1 | 1MHz | |
4.3 [-] Show Supplier Material materials with Dielectric constant of 4.3 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.5 [-] Show Supplier Material materials with Dielectric constant of 4.5 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
10 [-] Show Supplier Material materials with Dielectric constant of 10 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 20 kV/mm Show Supplier Material materials with Dielectric strength of 20 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Dielectric strength of 30 kV/mm | dry | IEC 60243-1 | ||
Dissipation factor | 60 [-] Show Supplier Material materials with Dissipation factor of 60 [-] | dry | IEC 62631-2-1 | 100Hz |
160 [-] Show Supplier Material materials with Dissipation factor of 160 [-] | dry | IEC 62631-2-1 | 1MHz | |
250 [-] Show Supplier Material materials with Dissipation factor of 250 [-] | dry | IEC 60250 | 1GHz | |
325 [-] Show Supplier Material materials with Dissipation factor of 325 [-] | conditioned | IEC 60250 | 1GHz | |
700 [-] Show Supplier Material materials with Dissipation factor of 700 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3300 [-] Show Supplier Material materials with Dissipation factor of 3300 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+08 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+08 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1470 g/cm³ Show Supplier Material materials with Density of melt of 1470 g/cm³ | dry | - | |
Shrinkage | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | dry | Sim. to ISO 294-4 | Parallel |
1.1 % Show Supplier Material materials with Shrinkage of 1.1 % | dry | Sim. to ISO 294-4 | Normal | |
Specific heat capacity melt | 1480 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1480 J/(kg·K) | dry | - | |
Spiral flow length | 105 | dry | - | 1.0 mm 800 bar |
115 | dry | - | 1.0 mm 900 bar | |
125 | dry | - | 1.0 mm 1000 bar | |
36 | dry | - | 0.5mm 1200 bar | |
50 | dry | - | 0.5mm 1600 bar | |
74 | dry | - | 0.5mm 2000 bar | |
Thermal conductivity of melt | 0.344 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.344 W/(m·K) | dry | - | |
Viscosity number | 145 cm³/gr Show Supplier Material materials with Viscosity number of 145 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Firefighter helmets, Miniature Circuit Breakers, Reflow connectors, FPC connectors, WtB and BtB Connectors, Battery Connectors, Thermostatic Controls, Hair Curler Brushes, Automotive Connectors, Endlaminates (electro motors), Brushholders (electro motors), Coil insulation, Automotive e-motor Bobbins, Molded case circuit breakers, Motor Starter/Overload Relays, Endlaminates (electrical components), Brushholders (electrical components), Bobbins, Reflow connectors (3) | |
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |