General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.45 g/cm³ Show Supplier Material materials with Density of 1.45 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Water absorption | 5.5 % Show Supplier Material materials with Water absorption of 5.5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 8 GPa Show Supplier Material materials with Elastic modulus of 8 GPa | conditioned | ISO 527-1/-2 | |
13 GPa Show Supplier Material materials with Elastic modulus of 13 GPa | dry | ISO 527-1/-2 | ||
Elongation | -40 °C | 3.1 % Show Supplier Material materials with Elongation of 3.1 % | dry | ISO 527-1/-2 |
3.3 % Show Supplier Material materials with Elongation of 3.3 % | dry | ISO 527-1/-2 | ||
6 % Show Supplier Material materials with Elongation of 6 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 12 GPa Show Supplier Material materials with Flexural modulus of 12 GPa | dry | ISO 178 | |
Flexural yield strength | 315 MPa Show Supplier Material materials with Flexural yield strength of 315 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry | ISO 179/1eA |
-30 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m² | dry | ISO 179/1eA | |
23 °C | 22 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 22 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 85 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 85 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 95 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 95 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | -40 °C | 285 MPa Show Supplier Material materials with Tensile strength of 285 MPa | dry | ISO 527-1/-2 |
140 MPa Show Supplier Material materials with Tensile strength of 140 MPa | conditioned | ISO 527-1/-2 | ||
205 MPa Show Supplier Material materials with Tensile strength of 205 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Heat deflection temperature | 210 °C Show Supplier Material materials with Heat deflection temperature of 210 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | UL746B | 0.71 mm | ||
Thermal diffusivity | 1.2e-07 mm²/s Show Supplier Material materials with Thermal diffusivity of 1.2e-07 mm²/s | dry | - | |||
Vicat softening temperature | 215 °C Show Supplier Material materials with Vicat softening temperature of 215 °C | dry | ISO 306 | 50°C/h 50N |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 500 V Show Supplier Material materials with Comparative tracking index of 500 V | conditioned | IEC 60112 | |
Dielectric constant | 3.3 [-] Show Supplier Material materials with Dielectric constant of 3.3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.4 [-] Show Supplier Material materials with Dielectric constant of 4.4 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
14.0 [-] Show Supplier Material materials with Dielectric constant of 14.0 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 25 kV/mm Show Supplier Material materials with Dielectric strength of 25 kV/mm | conditioned | IEC 60243-1 | |
35 kV/mm Show Supplier Material materials with Dielectric strength of 35 kV/mm | dry | IEC 60243-1 | ||
Dissipation factor | 50 [-] Show Supplier Material materials with Dissipation factor of 50 [-] | dry | IEC 62631-2-1 | 100Hz |
150 [-] Show Supplier Material materials with Dissipation factor of 150 [-] | dry | IEC 62631-2-1 | 1MHz | |
1100 [-] Show Supplier Material materials with Dissipation factor of 1100 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Dissipation factor of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1260 g/cm³ Show Supplier Material materials with Density of melt of 1260 g/cm³ | dry | - | |
Shrinkage | 0.34 % Show Supplier Material materials with Shrinkage of 0.34 % | dry | ISO 294-4 | Parallel |
0.83 % Show Supplier Material materials with Shrinkage of 0.83 % | dry | ISO 294-4 | Normal | |
Specific heat capacity melt | 2080 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2080 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.32 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.32 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Airbag Containers, Front End Modules | |
Certifications | Yellow Card Available | |
Fillers | 40% Glass Fiber |