Resistividad eléctrica: 1.83E-7 Ω·m

Quick Comparison

Acero bajo en carbono

EN 10025-2 Grade S235JR as-rolled condition (+AR)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Chromium Steel

ISO 683-3 Grade 16MnCr5 normalized or normalized formed (+N)

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Acero bajo en carbono

EN 10025-2 Grade S185 normalized or normalized formed (+N)

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00
Página 1 de 20